For amorphous materials, keep the bed near the glass transition temperature (Tg), within −10°C / +30°C.
For semicrystalline materials, use the filament manufacturer’s recommended bed temperature. If adhesion is a problem, the guidelines recommend printing near the melting temperature (Tm).
Use appropriate nozzle and chamber temperatures to reduce layer separation. Build plate adhesion has limits.
| Filament | First layer (°C) | Remaining layers (°C) | Part self-release |
|---|---|---|---|
| PSU | 175-195 | 165-195 | Releases easily after cooldown |
| PEI 9085 | 185-200 | 175-185 | Releases easily after cooldown |
| PEI1010 | 210-230 | 210-230 | Releases easily after cooldown |
| PPSU | 220-230 | 210+ | Releases easily after cooldown |
| PEKK | 175-185 | 175 | Releases easily after cooldown |
| LCP | 150-230 | 150+ | Releases easily after cooldown |
| PEEK | 230 | 230 | Releases easily after cooldown |
| PES | 230 | 230 | Releases easily after cooldown |
All temperatures are bed temperatures in °C. First layer and remaining layers are listed separately.
Source: Tyson Build Plates guidelines.